Argentium Sterling Silver Argentium Sterling Silver
 
Home Page
About Argentium Silver
Using Argentium Silver Casting Grain
Preventing Discoloration
Tips for Argentium Silver
Argentium Casting Grain
Argentium Flat Sheet
Argentium Hard Round Wire
Argentium 1/2 Hard Round Wire
Argentium Tubing
Argentium Half Round Wire
Argentium Square Wire
Argentium Solder
Argentium Jewelry Findings
Silver Refining
Silver Scrap
 

G&S METALS
gs@gsgold.com

 

PHONE
 
800.852.3860
+1.734-662-9344

 

ARGENTIUM™ SILVER CASTING GRAIN

DESCRIPTION: This is a new premium alloy which is more tarnish and perspiration resistant, whiter, easier to finish and has a higher melting temperature range.

FORM: Argentium® Silver casting grain comes as roughly spherical particles ranging from 1.75 to 4.75 mm in size.

ITEM NUMBER: SSCGAR

COMPOSITION: 97% Silver

DENSITY: 5.45 troy ounces/in3

SOLIDUS: 1522°F (828°C) LIQUIDUS: 1724°F (940°C)

CASTING: When investment casting, a pour temperature of 1780-1880°F
(950-980°C) and a flask temperature below 1350°F (677°C) are recommended. If casting without a protective atmosphere, the use of borax flux or graphite powder is effective. After casting the metal, a minimum of 15 minutes air cooling is recommended before quenching. Investment may be easily removed with water spray, ultrasound, and pickling solution.

HARDENING: Typical hardness of rapidly quenched pieces is 70 DPH.
Flasks cooled to room temperature can approach 90 DPH and heat-treated castings can approach 125 DPH! which is approximately twice the hardness of as-cast standard Sterling silver. To harden, quench the flask after air cooling for 15 minutes. Anneal in an oven at 1050°F to 1150°F (566°C-621°C) for 30-60 minutes and quench after visible heat has dissipated. Then, place the castings in an oven at 580°F (304°C) for 45 minutes and air cool to room temperature.

POLISHING: To avoid contamination from other alloys in the workshop, separate wheels should be used for Argentium® Sterling Silver. If this is not possible, thoroughly rake wheels before use.
After the final polishing, heat the castings in an air atmosphere to 250°F (121°C) for 20 minutes to activate the germanium oxide layer, which is highly tarnish resistant

REMELTING: Use at least a 50% fresh / 50% scrap mix. For higher quality pieces, using more fresh metal will yield superior results. It is important that used trees and buttons are free from investment powder residue, to avoid contamination.

WARRANTY CLAUSE: G&S Metals, Inc. believes this data to be accurate and reliable. However, these are recommendations only given free of charge and should be employed by you with discretion and risk. G&S Metals, inc. assumes no responsibility for difficulties or damages incurred by adhering to this information.

All Argentium Silver Jewelry Findings, Argentium Silver Casting Grain
and Argentium Mill Products prices in our shopping cart
are based on the London PM Fix and CHANGED DAILY.
Prices are subject to change without notice.

PURCHASE ARGENTIUM SILVER CASTING GRAIN, MILL PRODUCTS
AND ARGENTIUM SILVER JEWELRY FINDINGS ONLINE

ARGENTIUM SILVER IN STOCK AND READY FOR
IMMEDIATE SHIPPING !!

ALL PURCHASES MADE ON OUR SHOPPING CART ARE SECURE

Gallatin & Socha Metals
gs@gsgold.com